    Material Notes:
    
    Properties: Tungs ten-molybdenum high speed steel with ex cel lent toughness and cut ting proper ties, for a wide variety of uses.
    
    Applications:
    
    Taps, twist drills, reamers, broaching tools, metal saws, milling tools of all types, wood working tools, cold work tools.
| Physical Properties | |||
| Metric | English | Comments | |
| Density | 8.10 g/cc | 0.293 lb/in³ | |
| Mechanical Properties | |||
| Metric | English | Comments | |
| Modulus of Elasticity | 217 GPa | 31500 ksi | |
| Electrical Properties | |||
| Metric | English | Comments | |
| Electrical Resistivity | 0.0000540 ohm-cm | 0.0000540 ohm-cm | |
| Thermal Properties | |||
| Metric | English | Comments | |
| CTE, linear | 11.5 µm/m-°C | 6.39 µin/in-°F | |
| @Temperature 20.0 - 100 °C | @Temperature 68.0 - 212 °F | ||
| 11.7 µm/m-°C | 6.50 µin/in-°F | ||
| @Temperature 20.0 - 200 °C | @Temperature 68.0 - 392 °F | ||
| 12.2 µm/m-°C | 6.78 µin/in-°F | ||
| @Temperature 20.0 - 300 °C | @Temperature 68.0 - 572 °F | ||
| 12.4 µm/m-°C | 6.89 µin/in-°F | ||
| @Temperature 20.0 - 400 °C | @Temperature 68.0 - 752 °F | ||
| 12.7 µm/m-°C | 7.06 µin/in-°F | ||
| @Temperature 20.0 - 500 °C | @Temperature 68.0 - 932 °F | ||
| 12.9 µm/m-°C | 7.17 µin/in-°F | ||
| @Temperature 20.0 - 700 °C | @Temperature 68.0 - 1290 °F | ||
| 13 µm/m-°C | 7.22 µin/in-°F | ||
| @Temperature 20.0 - 600 °C | @Temperature 68.0 - 1110 °F | ||
| Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
| Thermal Conductivity | 19.0 W/m-K | 132 BTU-in/hr-ft²-°F | |
| Component Elements Properties | |||
| Metric | English | Comments | |
| Carbon, C | 0.85 % | 0.85 % | |
| Chromium, Cr | 4.1 % | 4.1 % | |
| Manganese, Mn | 0.25 % | 0.25 % | |
| Molybdenum, Mo | 5.0 % | 5.0 % | |
| Silicon, Si | 0.35 % | 0.35 % | |
| Tungsten, W | 6.4 % | 6.4 % | |
| Vanadium, V | 1.9 % | 1.9 % | |